It depends on if you want to restore it or return it to serviceable shooting condition. Because it's chambered for 38 special, I'd turn it into a shooter.
My choice considering the surface rust would be to glass bead blast it to make a satin surface then re-blue it. After a glass bead job, even cold blue refinish comes out great!
Flash
My choice considering the surface rust would be to glass bead blast it to make a satin surface then re-blue it. After a glass bead job, even cold blue refinish comes out great!
Flash