The press should come with 1 or 3. I think my single stage came with 3.I just realized what I forgot to order, breech lock bushings.
I wonder what else I forgot.
Sent from my LM-G820 using Tapatalk
The press should come with 1 or 3. I think my single stage came with 3.I just realized what I forgot to order, breech lock bushings.
I wonder what else I forgot.
Yes.Aren’t those like the LNL bushings?
You must have slept through math class.
2:1 is a ratio. You can make ANY size batch you want as long as you use two parts of one and one part of the other.
You are really splitting hairs. You get 13 and I get 12. Big deal. Water quench and you should get around 14 (in my experience). It's not that hard.2:1 is closer to 13 bhn. 3:1 is 11.7.
So 2 lbs of soft lead to every 1 lb of Linotype is NOT a 2:1 ratio?? lol ok, Leonard.
You are really splitting hairs. You get 13 and I get 12. Big deal. Water quench and you should get around 14 (in my experience). It's not that hard.
Oh, I see. It read like you were talking to me. My apologies.The person I responded to didn't know if a 2:1 ratio would fit in his 10 lb pot.
I rely on the measurement of the indention on the Lee table.I'm relying on an alloy calculator for my numbers. The calculator shows for a 2:1 ratio you should get 12.7, if you're rounding that's 13. Unless you work for the Government.
It's not that hard.
Friends-ish?Same team guys. This isn't Facebook. We're all friends here.
Sent from my LM-G820 using Tapatalk